We use the SAN material in the following processes:
- plastic injection moulding
- thermoplastic structure foaming (TSF)
SAN Material Datascheet:
特性 Property | 测试方法 Test Method | 测试条件Test Condition | 单位Unit | 一般注塑级SAN |
---|---|---|---|---|
引张强度 Tensile Strength | ASTM D638 |
1/8", 6 mm/min.
|
Kg/cm²
|
700
|
延伸率 Tensile Elongation | ASTM D638 |
1/8", 6 mm/min.
|
%
|
5.0
|
弯曲强度 Flexural Strength | ASTM D790 |
1/4", 2.8 mm/min.
|
Kg/cm²
|
1000
|
弯曲弹性率 Flexural Modulus | ASTM D790 |
1/4", 2.8 mm/min.
|
Kg/cm²
|
35000
|
IZOD冲击强度 IZOD Impact Strength | ASTM D256 (Notched) |
1/4", 23°C 1/8", 23°C |
Kg-cm/cm Kg-cm/cm |
1.7 1.8 |
流动系数 Melt Flow Index | ASTM D1238 |
200°C, 5 Kg
|
g/10min
|
2.8
|
硬度 Hardness | ASTM D785 |
1/4"
|
M Scale
|
83
|
密度 Density | ASTM D792 |
23°C
|
g/cm³
|
1.06
|
软化点 Vicat Softening Temp. | ASTM D1525 |
1/8", 50 °C/ hr
|
°C
|
102
|
热变形温度H.D.T Annealed(85°C, 8hr ) Unannealed | ASTM D648 |
1/4", 120 °C/ hr
|
°C
|
100 |
燃烧率 Flammability | UL94 |
–
|
–
|
HB
|